A study on the role of Ni content on structure and properties of Fe-Ni-Si-B-P-Cu nanocrystalline alloys
2021-09-02 14:18  

X.J. Jia, Y.H. Li, L.C. Wu, W. Zhang. Journal of Alloys and Compounds, 2020, 822:152784.

Abstract:

Amorphous-forming ability (AFA) and thermal stability of melt-spun Fe85-xNixSi2B8P4Cu1 (x = 0–20) alloys and their crystallized structure, magnetic and mechanical properties have been investigated. The increase of Ni content from 0 to 20 at.% gradually improves the AFA with enlarging the critical thickness for amorphous formation from 14 to 38 μm. Adding 5 at.% Ni increases the number density (Nd) of nucleation sites by properly delaying the Cu atoms clustering process during annealing and refines the α-(Fe, Ni) grains, which leads to a magnetic softness improvement of the nanocrystalline alloys. The excessive Ni (≥10 at.%) decreases the Nd due to the overinhibition of the Cu clustering, resulting in the grains coarsening and magnetic softness deterioration. The Fe80Ni5Si2B8P4Cu1 nanocrystalline alloy possesses finer α-(Fe, Ni) grains with an average size of 22 nm, a lower coercivity of 14.3 A/m and saturation magnetic flux density of 1.77 T as compared with those of 40 nm, 105.3 A/m and 1.84 T, respectively, for the Fe85Si2B8P4Cu1 alloy. In addition, the nanocrystalline alloys with 2.5–10 at.% Ni show reduced brittleness compared with the Ni-free alloy owing to the grain refinement, and the alloys with 15–20 at.% Ni possess further decreased brittleness as a consequence of the reduced α-(Fe, Ni) phase volume fraction.

详细

关闭窗口
 
 
 
 返回首页 | 网站地图 | 联系我们 | 管理登录 

大连理工大学非晶及纳米晶功能材料研究室  地址:辽宁省大连市大连理工大学材料科学与工程学院
电话:0411-84706400  邮编:116024